BRENNEN

Industries / Industrial equipment and services / Industrial services / Cathodic protection and corrosion control

Sacrificial anodes

Sacrificial, or galvanic, anodes are blocks of a more reactive metal, such as zinc, aluminum or magnesium, fixed or wired to the steel, which corrode in its place and need no power supply.

5

Milestones achieved, from 1824 to 2025.

1

To watch for: announced, not yet confirmed outside.

2

Open deliverables. Nobody has shipped them.

The road

AchievedWatch forOpen

Achieved

  1. 1824

    Iron guards a copper hull

    Humphry Davy, president of the Royal Society, found that small pieces of iron or zinc joined to copper sheathing stopped seawater eating the copper. In March 1824 cast iron "protectors" were fixed in four masses to the 28-gun HMS Samarang, which sailed to Nova Scotia and came back in January 1825. Davy, who saw her in dock, wrote that the copper was bright and almost free of weed, and called newspaper reports that her bottom was fouled "false and entirely unfounded". Ships given more iron did come back with barnacles, which Davy blamed on chalky deposits that the protection laid on the copper, and by the account of Ueli Angst of ETH Zurich the Royal Navy removed the protectors because protected copper no longer kept itself clean.

    LessonStopping a metal from dissolving also stops whatever good its dissolving did.

    archive.orgchemeurope.com

    Credit

    Humphry Davy, with Michael Faraday and the Royal Navy at Portsmouth

  2. 1945

    Magnesium for buried pipe

    Magnesium gives about 1,000 ampere-hours of current per pound in theory, against 372 for zinc, and pushes a stronger current through soil, Chemical & Engineering News reported in 1945. Porter Hart and Yale W. Titterington reported in the first volume of the journal Corrosion (1945) that at 200 milliamperes per square foot only about half the metal gave useful current; the rest was lost to the anode corroding itself, and its impurities and the backfill packed around it decided how much. In 1941 the National Bureau of Standards had buried zinc-iron couples at eight sites to test zinc in soil, and at one of them protection was not adequate.

    LessonAn anode's real output is set by its impurities, its backfill and the current asked of it, not by its chemistry alone.

    nvlpubs.nist.govdoi.org

    Credit

    Porter Hart and Yale W. Titterington; Melvin Romanoff (National Bureau of Standards)

  3. 2008

    Hydrogen cracks duplex steel

    Duplex stainless steels, a strong, corrosion-resistant family used for subsea hubs, pipes and valve bodies, had "some significant failures" under cathodic protection, DNV wrote in its recommended practice DNV-RP-F112 of October 2008. The cause was hydrogen, formed on the steel surface by the protection itself, entering highly stressed metal. Laboratory tests showed duplex steels susceptible at potentials more negative than about −850 mV against a silver/silver chloride electrode, and full-scale tests failed at lower stress than small specimens. DNV's anode design practice, DNV-RP-B401, also records cracking from protection in martensitic steels with a yield strength of about 700 MPa and a hardness of 350 HV.

    LessonThe protecting current makes hydrogen, so strong or hard steels need limits on stress and hardness when they are protected.

    rules.dnv.comrules.dnv.com

    Credit

    DNV (Det Norske Veritas)

  4. 2024

    Retrofit anodes acidify monopiles

    A monopile is the single large steel tube, driven into the seabed, that carries most offshore wind turbines. Early designs counted on the water sealed inside going stagnant and losing its oxygen, so the inside needed no protection; leaking seals, water seeping through the seabed and decks that were not airtight let corrosion go on, and aluminum anodes were fitted inside afterwards. Where the water barely changed, those anodes turned it acid, from about pH 8 to below pH 4 within weeks. Laboratory tests by Intertek CAPCIS found the pH fell sharply once dissolved aluminum passed about 10 mg/L, while zinc anodes left the pH steady. DNV-RP-0416 (2021) and ISO 24656 (2022) now cover inside surfaces.

    LessonAn anode that works in the open sea can harm a closed space, because its corrosion products stay put.

    icorr.org

    Credit

    David Buxton, Gareth John, J. D. Stott and Petra Ernst of Intertek CAPCIS, presented to the Institute of Corrosion in April 2024

  5. 2025

    Indium traces wind farm anodes

    Aluminum anodes for the sea contain small amounts of zinc and indium, and indium hardly occurs in seawater otherwise. Researchers at the Helmholtz-Zentrum Hereon in Germany analyzed 235 surface water samples taken in German North Sea offshore wind farms between 2016 and 2022 for 32 metals. Raised indium may be linked to the farms' corrosion protection, they found, while the other metals stayed within natural variation. A companion study of mussels growing on turbine foundations found no noteworthy uptake of anode metals.

    ebi.ac.ukebi.ac.uk

    Credit

    Anna Ebeling, Daniel Pröfrock and colleagues (Hereon); Alexa Zonderman and colleagues

Watch for

  1. Metal released per monopile

    Researchers modeled galvanic anode protection of offshore wind monopiles over a 25-year life, compared the model with field data, and estimated that 20% to 36% of the anode mass ends up released as metal, giving concentrations of 0.091 to 0.111 ppm aluminum and 0.005 to 0.006 ppm zinc. They say these are well above natural background but 11 to 13 times below reported toxicity limits for aluminum and 6 to 8 times below those for zinc.

    Achieved whenwater and sediment sampling around a monopile wind farm, by a group outside the study, measures concentrations in the predicted range.

    tethys.pnnl.gov

    Claimed by

    Mohammad Afshari of the Technical University of Denmark, Mehdi Attarchi of Vattenfall, an operator, and colleagues, in Materials and Corrosion, December 2025

Open

  1. 01

    Test anodes for a year

    A public, twelve-month test of aluminum-zinc-indium anodes bought on the open market from at least five makers. Each anode is joined to a bare steel plate in a tank of seawater at the low current a real anode gives, with its current and potential logged throughout and its weight loss measured at the end, so that its capacity in ampere-hours per kilogram can be set beside its maker's figure.

    The brief
    Credit · unclaimed
  2. 02

    Weigh anodes from retired platforms

    A public table of the galvanic anodes taken off decommissioned offshore platforms and subsea structures as they reach recycling yards. Each anode is cleaned, weighed and photographed and recorded with its structure, its install year and its position, and the metal left is compared with what the design expected to be left.

    The brief
    Credit · unclaimed

Open 01 · the brief

Test anodes for a year

Credit · unclaimed

The first to publish is credited on this line, and the deliverable moves from Open to Achieved.

What to build

A public, twelve-month test of aluminum-zinc-indium anodes bought on the open market from at least five makers. Each anode is joined to a bare steel plate in a tank of seawater at the low current a real anode gives, with its current and potential logged throughout and its weight loss measured at the end, so that its capacity in ampere-hours per kilogram can be set beside its maker's figure.

Why it is still open

DNV's design practice warns that short laboratory tests "will typically result in values close to the theoretical limit (e.g. 2,500 Ah/kg for Al-Zn-In material)" because they run at high current, tells designers to use lower default values unless long-term tests justify more, and says a maker's test data must match the alloy and casting actually supplied. The nearest outside comparison found, by Petrobras engineers in 1999, ran anodes from four makers for six months in seawater and two marine soils, in a paywalled journal. A 2023 neural-network study predicts anode efficiency from published laboratory data rather than new long tests.

rules.dnv.comosti.govgithub.com

Built with what exists

Polyethylene tanks of natural seawater or substitute ocean water made to ASTM D1141; mild steel plates; shunt resistors read by a small data logger, such as a Raspberry Pi with an ADS1115 converter board; silver/silver chloride reference electrodes; a balance reading to 0.01 g; the long-term test procedure in Annex C of DNV-RP-B401; anodes bought from distributors.

  1. First step

    Buy one anode from each of two makers, cut matched samples, and run a four-week trial in two tanks to prove the logging and the weighing.

  2. Done looks like

    Twelve months of logged current for at least 15 anodes, three from each of five makers, with capacity and efficiency for each anode and their uncertainty, each maker's result set beside its datasheet, and the raw data released under an open license.

Open 02 · the brief

Weigh anodes from retired platforms

Credit · unclaimed

The first to publish is credited on this line, and the deliverable moves from Open to Achieved.

What to build

A public table of the galvanic anodes taken off decommissioned offshore platforms and subsea structures as they reach recycling yards. Each anode is cleaned, weighed and photographed and recorded with its structure, its install year and its position, and the metal left is compared with what the design expected to be left.

Why it is still open

Remaining anode life is judged in place, by cleaning anodes under water and estimating their size. At Ghana's Jubilee field more than 430 anodes were cleaned this way for a 2018 survey. Shell and TWI's study of the five Indefatigable platforms in the southern North Sea, installed between 1970 and 1986 and retrieved by June 2011, set out to measure their steels and fatigue lives, and its findings go to paying sponsors.

offshore-mag.comtwi-global.com

Built with what exists

A crane scale and a bench scale; a pressure washer; a camera; public decommissioning programmes and close-out reports, such as those the UK regulator OPRED posts on gov.uk; an AI model to pull install years and anode details out of long PDF reports (see the Note "The jobs agents repeat"); the anode utilization factors in DNV-RP-B401 for the comparison.

  1. First step

    Ask one decommissioning yard for leave to weigh, with its own staff doing the lifting, the anodes from one structure already ashore, and check whether that structure's decommissioning programme lists its anode tonnage.

  2. Done looks like

    At least 300 anodes from at least five structures weighed, 10% of them weighed again by a second person, and the measured remaining mass for each structure set against its design figure.