BRENNEN

Industries / Industrial equipment and services / Industrial machinery / Fasteners

Coating

Coating puts a thin layer, usually zinc or a zinc alloy, on a finished fastener so that it does not rust, and a topcoat over it often sets how much friction the thread has when the fastener is tightened.

4

Milestones achieved, from 1974 to 2007.

1

To watch for: announced, not yet confirmed outside.

2

Open deliverables. Nobody has shipped them.

The road

AchievedWatch forOpen

Achieved

  1. 1974

    Zinc flakes without plating

    Zinc flake coatings are a water-based mix of overlapping zinc and aluminium flakes in a binder, applied without electroplating; their maker lists the process as free of hydrogen embrittlement. Metal Coatings International, part of the NOF Metal Coatings group, says the group originated zinc flake coatings in 1974. Its earlier Dacromet finish held a trace of hexavalent chromium.

    pfonline.comsurfacefinishing.com

    Credit

    NOF Metal Coatings group, by its own account

  2. 1980s

    Galvanized strong bolts crack

    Hot-dip galvanizing cleans steel in acid and then dips it in molten zinc. The American Galvanizers Association (AGA) says research in the late 1970s and early 1980s found failure rates of up to 25% among hot-dip galvanized ASTM A490 bolts, structural bolts with a tensile strength of 150 to 173 ksi, and that ASTM then excluded metallic coatings from them except approved zinc-aluminium coatings. The Research Council on Structural Connections' 2020 specification still does not permit zinc on these bolts, now graded ASTM F3125 Grade A490, because "its effects on embrittlement and delayed cracking have not been fully investigated to date".

    LessonThe AGA traces the hydrogen to the acid cleaning before the zinc bath; a step that is harmless to an ordinary bolt can crack one above about 150 ksi.

    galvanizeit.orggalvanizeit.org

    Credit

    ASTM; Research Council on Structural Connections (the AGA does not name the researchers)

  3. 1991

    Europe limits cadmium plating

    EU Council Directive 91/338/EEC of 18 June 1991 banned cadmium plating on equipment for food production, agriculture, refrigeration, printing and many other uses, and on road vehicles, rolling stock and ships. It exempted products for the aeronautical, aerospace, mining, offshore and nuclear sectors, safety devices in vehicles, rolling stock and ships, and electrical contacts. Member states had to apply it by 31 December 1992.

    eur-lex.europa.eu

    Credit

    Council of the European Communities

  4. 2007

    Carmakers drop chromate coatings

    The EU End-of-Life Vehicles Directive (2000/53/EC) banned lead, mercury, cadmium and hexavalent chromium, a toxic form of chromium, from materials and components of vehicles put on the market after 1 July 2003, with exceptions listed in an annex: corrosion-preventive coatings could keep hexavalent chromium until 1 July 2007, and coatings on bolt and nut assemblies for chassis until 1 July 2008. Metal Coatings International says it had moved its North American customers from Dacromet to the chromium-free Geomet by 1 July 2002.

    eur-lex.europa.eueur-lex.europa.eupfonline.com

    Credit

    European Parliament and Council; European Commission

Watch for

  1. PFAS-free friction topcoats

    Zinc flake topcoats commonly use fluoropolymers such as PTFE as a lubricant that sets how a bolt tightens. PTFE belongs to PFAS, a large family of long-lasting fluorine chemicals on which a European Commission decision is still pending. Dörken says its PFAS-free topcoat DELTA-PROTEKT TC 502 GZ has been approved under Volkswagen's specification VW TL245 Ofl-t647, and calls this the first global approval of a PFAS-free system in the automotive industry. Its datasheet for another PFAS-free topcoat, TOP 500 BLACK, gives a friction coefficient window of 0.08 to 0.14 under ISO 16047, measured on M10 bolts with Dörken's own basecoat.

    Achieved whenVolkswagen or another carmaker confirms series use, or an outside lab publishes friction results across several lots that fall inside the stated window.

    doerken.comipcm.itdoerken.com

    Claimed by

    Dörken, January 2026

Open

  1. 01

    Coating claims, tested independently

    An outside test of the friction and corrosion figures that coating makers print, on one bolt size with six commercial systems, including zinc flake with a PTFE topcoat, zinc flake with a PFAS-free topcoat, zinc-nickel plating, and zinc plating with a thick trivalent passivate.

    The brief
    Credit · unclaimed
  2. 02

    Galvanized A490 tested openly

    A published test of ASTM F3125 Grade A490 bolts that are hot-dip galvanized after blast cleaning instead of acid cleaning, the change the AGA says removes the source of hydrogen, with uncoated and zinc-aluminium coated bolts as controls. An accredited lab runs ASTM F1624, the incremental step-load test for hydrogen embrittlement, and the test bolts are scrapped afterwards, never used in a structure.

    The brief
    Credit · unclaimed

Open 01 · the brief

Coating claims, tested independently

Credit · unclaimed

The first to publish is credited on this line, and the deliverable moves from Open to Achieved.

What to build

An outside test of the friction and corrosion figures that coating makers print, on one bolt size with six commercial systems, including zinc flake with a PTFE topcoat, zinc flake with a PFAS-free topcoat, zinc-nickel plating, and zinc plating with a thick trivalent passivate.

Why it is still open

Friction windows and salt spray hours come from the coating makers, measured on their own test parts: Dörken's 0.08 to 0.14 window on its own basecoat, and 500 to 720 hours of salt spray for Geomet from Metal Coatings International. ISO/TR 19852, published in February 2026, reports an interlaboratory test of the neutral salt spray method on zinc and zinc-nickel plated bolts; it tests the method, not the makers' claims. Searches found no independent comparison of commercial fastener coatings.

doerken.comsurfacefinishing.comdin.de

Built with what exists

Bolts bought through ordinary distributors; two labs accredited to ISO/IEC 17025, one for friction tests under ISO 16047 and both for neutral salt spray under ISO 9227; Python for the statistics.

  1. First step

    Choose the six systems, buy one lot of each from two distributors, and get quotes from two accredited labs.

  2. Done looks like

    Six systems with three lots each, at least 10 friction tests per lot with the measured range set beside each claimed window, salt spray hours to white rust and to red rust from both labs, and all raw data published.

Open 02 · the brief

Galvanized A490 tested openly

Credit · unclaimed

The first to publish is credited on this line, and the deliverable moves from Open to Achieved.

What to build

A published test of ASTM F3125 Grade A490 bolts that are hot-dip galvanized after blast cleaning instead of acid cleaning, the change the AGA says removes the source of hydrogen, with uncoated and zinc-aluminium coated bolts as controls. An accredited lab runs ASTM F1624, the incremental step-load test for hydrogen embrittlement, and the test bolts are scrapped afterwards, never used in a structure.

Why it is still open

ASTM and the Research Council on Structural Connections still do not permit galvanized A490 bolts. The AGA says its 2013 study, published in a trade magazine, showed the modified process is feasible and that European galvanizers use it, and wrote in 2021 that an ASTM subcommittee ballot to allow it was under way. A search found no approved change and no public data set.

galvanizeit.orggalvanizeit.orgstore.astm.org

Built with what exists

A490 bolts from two makers; three commercial galvanizers, each paid to blast-clean and galvanize one batch as an ordinary job; a lab accredited to ISO/IEC 17025 with incremental step-load equipment; the AGA's published process description.

  1. First step

    Ask the AGA for the raw data from its 2013 study, and get quotes from two galvanizers for blast-cleaned galvanizing of 1-inch A490 bolts.

  2. Done looks like

    At least 30 bolts per group from each of the three galvanizers, plus the controls, with threshold loads and any delayed fractures published and the results sent to ASTM Committee F16 as public data.